- The main chemical composition of the mixture includes 04 main oxides such as: CaO limestone, and SiO2, Fe2O3, Al2O3 clay, if it is lacking, it will be supplemented with the above adjustment additives.
- 04 main oxides in the mixture when heated to 1450 degrees C will react with each other to form 4 main minerals in C3S 3CaO clinker. SiO2; C2S2Cao.SiO2; C3A 3CaO.Al2O3; C4AF 4CaO. Al2O3. Fe2O3
These minerals have different crystal structures and determine the quality of the clinker. The quality of the clinker will determine the quality of the cement.
Quantity:
2018: 3 Million Tons
2019: 2,7 Million Tons
2020: 2,8 Million Tons
2021: 2,9 Million Tons
Supply capacity:
Loading/Discharging rate: 8,000 – 15,000 MT/day
We can handle all sizes of vessels that is suitable for loading/discharging ports
Supply capacity upto 400,000MT/month
Main loading/discharging ports:
Cam Pha port – Quang Ninh province
Hon Gai port – Quang Ninh province
Hai Phong port – Hai Phong city
Nghi Son port – Thanh Hoa province
Vissai port – Thanh Hoa province
Chan May port – Thua Thien Hue
Thuan An port – Thua Thien Hue
Soai Rap port – Ho Chi Minh City